MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Plaskolite Optix® CA-924 G PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Availability: North America

Features: Electrically Insulating; Good Impact Resistance; Good Weather Resistance; Machinable; Radiation Sterilizable

Uses: Medical/Healthcare Applications

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Injection Molding

Information provided by Plaskolite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0070 cm/cmASTM D955
Melt Flow 6.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 68ASTM D785
Tensile Strength, Yield 8470 psiASTM D638
Elongation at Break 4.5 %ASTM D638
Tensile Modulus 472000 psiASTM D638
Flexural Yield Strength 12500 psiASTM D790
Flexural Modulus 370000 psiASTM D790
Compressive Strength 12000 psiASTM D695
Izod Impact, Notched 0.800 ft-lb/inASTM D256
Gardner Impact 14.0 in-lbASTM D3029
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.44
@Frequency 1e+6 Hz
ASTM D150
 3.14
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 380 V/milASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz
ASTM D150
 0.041
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 182 °FUnannealed; ASTM D648
Vicat Softening Point 233 °FASTM D1525
UL RTI, Electrical 122 °F
@Thickness 1.52 mm
UL 746B
UL RTI, Mechanical with Impact 122 °F
@Thickness 1.52 mm
UL 746B
UL RTI, Mechanical without Impact 122 °F
@Thickness 1.52 mm
UL 746B
Flammability, UL94 HB
@Thickness 1.52 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Transmission, Visible 91.6 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 350 - 450 °F
Middle Barrel Temperature 380 - 480 °F
Front Barrel Temperature 400 - 500 °F
Nozzle Temperature 380 - 480 °F
Melt Temperature 420 - 480 °F
Mold Temperature 110 - 190 °F
Drying Temperature 180 °F
Dry Time 2.00 - 4.00 hour
Injection Pressure 10000 - 20000 psi
Back Pressure 50.0 - 150 psi
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLASKO839 / 311532

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.