- Super soft EPDM crushed (semi-closed cell) foam.
- UL 94 5VA, V-0 HF-1 listed for flame
- Meets Toyota TSK 6505F Class 2A
- Manufactured in continuous rolls
- Excellent resistance to ozone, weathering and heat
- ASTM E-84 (25/50 Rated)