System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Novamid® 1013GH15 1 NA/BK37 PA6-GF15
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 20% Glass Fiber Filled
Material Notes:
15% Glass Reinforced, Heat Stabilized, Injection Molding
Former DSM Engineering Plastics product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.23
g/cc
dry; ISO 1183
Moisture Absorption
3.00 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow
0.0040
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.013
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
70.0
MPa
cond; ISO 527-1/-2
130
MPa
dry; ISO 527-1/-2
Elongation at Break
2.7 %
dry; ISO 527-1/-2
8.7 %
cond; ISO 527-1/-2
Tensile Modulus
2.80
GPa
cond; ISO 527-1/-2
5.80
GPa
dry; ISO 527-1/-2
Flexural Strength
115
MPa
cond; ISO 178
200
MPa
dry; ISO 178
Flexural Modulus
2900
MPa
cond; ISO 178
5400
MPa
dry; ISO 178
Charpy Impact Unnotched
39.0
kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eU
106
kJ/m²
@Temperature 23.0 °C
cond; ISO 179/1eU
Charpy Impact, Notched
6.00
kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eA
14.0
kJ/m²
@Temperature 23.0 °C
cond; ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
6.00e+14
ohm-cm
dry; IEC 60093
Surface Resistance
8.00e+13
ohm
cond; IEC 60093
Dielectric Constant
4.0
@Frequency 100 Hz
dry; IEC 60250
4.0
@Frequency 1e+6 Hz
dry; IEC 60250
Dielectric Strength
27.0
kV/mm
dry; IEC 60243-1
Dissipation Factor
0.013
@Frequency 100 Hz
dry; IEC 60250
0.023
@Frequency 1e+6 Hz
dry; IEC 60250
Comparative Tracking Index
400
V
dry; IEC 60112
Thermal Properties
Original Value
Comments
Melting Point
220
°C
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
216
°C
dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
194
°C
dry; ISO 75-1/-2
Flammability, UL94
HB
@Thickness 0.800 mm
dry; IEC 60695-11-10
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Akulon® K224-PG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)
Envalior Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
PDSM9868 / 161489
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.