MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Bapolene PP4012F is a homopolymer polypropylene (flake) that meets US FDA 21CFR177.1520.

Applications: Color Concentrates; Compounding.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Food Contact Acceptable; Homopolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D-785
Tensile Strength, Yield 34.1 MPaASTM D-638
Elongation at Yield 10 %ASTM D-638
Flexural Modulus, 1% Secant 1.434 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 119 °CASTM D-648
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
Overview of materials for Polypropylene, Extrusion Grade
Bamberger Polymers Bapolene® 4052F Polypropylene, Blown Film Grade
Mitsubishi Chemical Advanced Materials Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Bamberger Polymers Bapolene® 4042 Polypropylene, Fiber/Filament Grade

PBP3B170F / 177707

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.