Description: Flow media. Ideally suited to infusion applications. Features & Benefits: - Open polyethylene mesh suitable for resin infusion processing.
- The open 3.175 mm (0.125 in) diamond mesh allows for easy flow of resin to ensure complete substrate saturation during the infusion process.
- Compatible with most commonly used infusion resins.
- Will not fray when cut, and lays flat on fooling and part surfaces.
Information provided by Cytec, subsequently acquired by Solvay. |