SABIC® PP customized solution (CS) is a concept based on a reactor elastomer-modified PP combined with a talcum filled masterbatch mixed at the injection-molding machine. SABIC® PP CS offers a low cost customized solution. The SABIC® PP CS concept offers optimal flexibility by creating the possibility to correct dimensions, if needed, in a fast, reliable and accurate way without affecting material logistics. This properties table contains typical values for SABIC® PP CS systems with 40% talcum masterbatch resulting in a material with 20% talcum. The polymer used is SABIC® PP 95610 and the masterbatch is the SABIC® PP compound 20MBT.
IMDS ID: 16487435Information provided by SABIC |