MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco NLGI 2 Moly Grease EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Features

Chevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybdenum disulfide (moly), EP additive, rust and oxidation inhibitors. They are dark gray/black in color and smooth and buttery in texture.

These products satisfy the demand for high quality moly-type greases with extreme pressure capability in both automotive and industrial applications.

Chevron Moly Greases EP provide excellent performance under extreme pressure, boundary lubrication conditions because of their EP additive and moly content. With a Timken OK Load (ASTM D 2509) of 50 lbs and moly to maintain a low coefficient of friction along sliding surfaces, even under loads exceeding the yield strengths of metals, Chevron Moly Greases EP provide both shock and heavy load protection. Moly provides a lubricity safety factor (staying power) in situations where the grease is depleted and only molybdenum disulfide remains to provide lubrication until more grease is applied.

Chevron Moly Greases EP provide longer-lasting lubrication than conventional greases. Hence, lubrication frequencies can be extended and down time reduced. They are ideal in situations where lubrication is infrequent. The "moly" provides a reserve protection should the lubricant be squeezed from the bearing surface. They have good storage stability, are pumpable at low temperatures, and provide water resistance and rust protection.

Applications

Chevron Moly Greases EP are recommended for use in automotive and industrial equipment where a moly type grease is called for.

Typical applications in automotive equipment are: chassis, bearings, universal joints, fifth wheels, and ball joints in construction equipment such as bulldozers, scrapers, loaders, shovels, etc.

Chevron Moly Greases EP are recommended for use in roller chains, trunions, gears, cables, sheaves, slides, and chassis bearings.

In industrial applications, these greases are recommended for the lubrication of conveyor bearings, sliding and rubbing surfaces, kiln car bearings, etc. They are particularly suited for heavily loaded pivot pins, splined shafts, or other surfaces subjected to sliding, vibration, or oscillation where fretting is encountered.

Chevron Moly Greases EP meet Caterpillar recommendations for greases containing 3% molybdenum disulfide.

Key Words: CPS Number: 255660; MSDS Number: 6912
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 53Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1074 SUS
Saybolt Viscosity at 210°F 77 SUS
Kinematic Viscosity at 40°C (104°F) 200 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 14.2 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kgWeld Point
Penetration 280Worked
Penetration P(0), 1/10 mm 275
Timken Test 50.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 127 °C
Minimum Service Temperature, Air -15.0 °C
Pour Point -18.0 °CASTM D97
Flash Point 249 °CASTM D92
Dropping Point 191 °C
 
Descriptive Properties
ColorDark Gray/Black
Lincoln Ventmeter, psig at 30 s, at 0°F583
Lincoln Ventmeter, psig at 30 s, at -22°F1367
Lincoln Ventmeter, psig at 30 s, at 75°F400
TextureSmooth, Buttery
Thickener, % / type6.4 / Lithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV255 / 74870

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.