Ateva® 1231 resin is designed for medical and other tubing applications, it is also well suited for high quality microcellular crosslinked foam applications. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: Applications: Foam; Medical; Tubes & Pipes Information provided by Celanese Corporation. |
medical and other tubing applications; high quality microcellular crosslinked foam |