System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® BKV 30 EF 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Glass Fiber Filled
Material Notes:
PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow)
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.35
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.0017
cm/cm
150x105x3; ISO 2577
0.0023
cm/cm
60x60x2; ISO 2577
Linear Mold Shrinkage, Transverse
0.0058
cm/cm
60x60x2; ISO 2577
0.0074
cm/cm
150x105x3; ISO 2577
Melt Flow
75
g/10 min
@Load 5.00 kg,
Temperature 270 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
190
MPa
ISO 2093-1
Tensile Strength at Break
180
MPa
5 mm/min; ISO 527-1,-2
Elongation at Break
3.2 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
9300
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
270
MPa
2 mm/min; ISO 178-A
Flexural Yield Strength
255
MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
7800
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
4.1 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
55.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched
50.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
65.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
<=
12.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Electrical Properties
Original Value
Comments
Comparative Tracking Index
550
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
20.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
100
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point
220
°C
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
210
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
150
°C
ISO 75-1,-2
Vicat Softening Point
>=
210
°C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94
HB
@Thickness 0.750 mm
Shrinkage, MD
0.040 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 2577
Shrinkage, TD
0.14 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 2577
0.15 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 2577
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
Mold Temperature
80.0
°C
Back Pressure
50.0
MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLANW9528 / 208199
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.