MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Kraton® D1116 K (SBS) Radial Triblock Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified:
Kraton D1116 KT - supplied as a dusted porous pellet
Kraton D1116 KU - supplied as an undusted porous pellet
Kraton D1116 KIM - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1116 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Note 1) The final dusting level is a combination of the talc from the original D1116 KT plus PGA-SD Alumina added during the milling process

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D4025
Volatiles <= 0.70 %KM 04
Viscosity 2000 - 3000 cP20% Toluene Solution at 25°C; BAM 922
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Ash 0.15 - 0.35 %KT, Talc; BAM 908
 3.0 - 5.0 %TIM, See Note 1); BAM 908
 
Chemical PropertiesOriginal ValueComments
Diblock Content 16 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63
@Time 10.0 sec
Typical values on polymer compression molded at 350°F; ASTM D2240
Tensile Strength 31.7 MPaTypical properties of film cast from toluene solution; ASTM D412
Elongation at Break 900 %Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.00241 GPa
@Strain 300 %
film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.15-0.4%, KM 08
 Polystyrene21.1-24.4%, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber Ratio23/77

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® FG1901 + PBT blend (30/70)
Kraton® D1102 B (SBS) Liner Block Copolymer
Kraton® D1101 E (SBS) Liner Block Copolymer
Kraton® D1102 J (SBS) Liner Block Copolymer
Kraton® D1102 E (SBS) Liner Block Copolymer

PKRA9815 / 132714

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.