MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin NH6010B Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NH6010B resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high performance, injection moldable and extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 1.5mm. NORYL NH6010B resin features low smoke production upon burning, high heat resistance, very low specific gravity, and compliance to IEC. In addition, this material is heat stabilized and impact modified. It is an excellent candidate for conduit and trunking applications in transportation, building + construction, and electrical markets. *see NORYL LS6010 resin for FAR 25.853 requirements.

Features: Hydrolytic Stability,Low Smoke and Toxicity,Low Creep Sensitivity,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Moisture Absorption 0.0500 %23°C / 50% RH; ISO 62
 0.0700 %Profile Extrusion
 0.0700 %Sheet Extrusion
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 5.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 5.6 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.0 MPa50 mm/min; ASTM D638
 58.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa50 mm/min; ASTM D638
 64.0 MPa50 mm/min; ISO 527
Elongation at Break 8.3 %50 mm/min; ISO 527
 20 %50 mm/min; ASTM D638
Elongation at Yield 4.6 %50 mm/min; ASTM D638
 4.7 %50 mm/min; ISO 527
Tensile Modulus 2220 MPa5 mm/min; ASTM D638
 2440 MPa1 mm/min; ISO 527
Flexural Strength 100 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 100 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2360 MPa2 mm/min; ISO 178
 2390 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 300 JASTM D256
 181 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 18.0 kJ/m²80*10*4; ISO 180/1A
 14.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 20.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 52.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.62e+17 ohm-cmASTM D257
 7.62e+17 ohm-cmIEC 60093
Surface Resistance 1.25e+18 ohmASTM D257
 1.25e+18 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.78
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 34.1 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 34.1 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0029
@Frequency 1e+6 Hz
ASTM D150
 0.0029
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 143 °CRate B/50; ASTM D1525
 143 °CRate B/50; ISO 306
 146 °CRate B/120; ISO 306
Smoke Density 7.0
@Thickness 1.52 mm
Non-Flaming, 4 min; ASTM E662
 30
@Thickness 1.52 mm
Flaming, 4 min; ASTM E662
 30
@Thickness 3.20 mm
Flaming, 4 min; ASTM E662
 120
@Thickness 3.20 mm
Flaming, 20 min; ASTM E662
Oxygen Index 33 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 30.0 - 50.0 °CWater Bath Temperature
 30.0 - 60.0 °CCalibrator Temperature
Nozzle Temperature 295 - 305 °C
Zone 1 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
Zone 2 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
 290 - 300 °C
Zone 3 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
 295 - 305 °C
Zone 4 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
Adapter Temperature 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
Die Temperature 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
Melt Temperature 220 - 260 °CProfile Extrusion
 220 - 260 °CSheet Extrusion
 280 - 305 °CInjection Molding
Mold Temperature 65.0 - 100 °C
Roll Temperature 90.0 - 150 °CRoll Stack Temp - Bottom
 90.0 - 150 °CRoll Stack Temp - Middle
 90.0 - 150 °CRoll Stack Temp - Top
Drying Temperature 95.0 - 105 °CInjection Molding
 95.0 - 105 °CProfile Extrusion
 95.0 - 105 °CSheet Extrusion
Dry Time 2.00 - 4.00 hourInjection Molding
 2.00 - 4.00 hourProfile Extrusion
 2.00 - 4.00 hourSheet Extrusion
 12.0 hourCumulative; Injection Molding
 12.0 hourCumulative; Profile Extrusion
 12.0 hourCumulative; Sheet Extrusion
Shot Size 30 - 70 %
Screw Speed 40 - 80 rpm
Precipitation Temperature 80.0 - 120 °CHopper Temperature
 
Descriptive Properties
Ds_4min70ISO 5659-2
F1 Class Smoke and Toxicity Rating3 mmNF F16-101
Flame Spread Index (1.52mm)15ASTM E162
Heat Release, MAHRE33.6 kW/m²ISO 5660-1
Lateral Flame Spread, CFE20 kW/m²ISO 5658-2
M1 Flame Class Rating2 mmNF P 92501
Toxicity0ISO 5659-2
Toxicity (3 mm)21.76NF X70-100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82393 / 290340

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.