MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Canadian Wear Technologies Abreco ASTM A-532 Class II Type B Laminated Abressive Resistant High Chromium Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; White Cast Iron

Material Notes: Proprietary grade of high chrome white iron brazed to a mild steel backer plate. This results in a final product that has superior wear and abrasion resistance while also being tough. Abreco plate is often used in high wear applications such as apron feeders, vibratory feeders, chutes, conveyors, crushers, hoppers, transfer points and buckets - to mention a few. The mild steel backing plate also facilitates the welding of a variety of mounting systems, allowing Abreco plate to be installed on any surface. Abreco plate has a hardness of approximately 650 HB or 62/64 Rc and can be cast in variety of custom shapes and sizes to meet the needs of any application.

Information provided by Canadian Wear Technologies.

Key Words: ASTM A-532, ASTM A-532 Class II Type B, AR400, AR Cast Iron, Laminated Wear Plate, High Chromium Cast Iron, High Chrome White Iron, CWI, HCWI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 486 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 450anealed and normalized
 650Typical
 800quenched
Hardness, Rockwell C 45anealed and normalized
 58Typical
 64quenched
Modulus of Elasticity 200 - 250 GPa
Compressive Yield Strength 220 - 480 MPaVaries by heat treatment cycle and chemistry
Compressive Strength 230 - 480 MPaDependent on the the heat treatment cycle
Charpy Impact 30.0 - 40.0 JVaries significantly by temperature and mechanical design / lamination configuration
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 10.0 - 500 °C
Thermal Conductivity 8.50 - 18.0 W/m-KVaries by temperature
Melting Point 1350 °CTypical, dependent on chemistry and grade
 1270 - 1430 °CRange, dependent on chemistry and grade
Solidus 1270 °C
Liquidus 1430 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.0 - 3.3 %
Chromium, Cr 14 - 18 %
Copper, Cu 0.0 - 1.2 %
Manganese, Mn 0.2 - 2 %
Molybdenum, Mo 0.0 - 3 %
Nickel, Ni 0.0 - 2.5 %
Phosphorus, P <= 0.05 %
Silicon, Si 0.3 - 1.5 %
Sulfur, S <= 0.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NCWT990 / 287909

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.