MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Azoty Tarnow™ TARNOFORM 200 HI4 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Rubber modified grade with very high impact strength and damping capacity.

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183
Melt Flow 2.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ISO 2039-2
Ball Indentation Hardness 82.0 MPa358 N; ISO 2039-1
Tensile Strength, Yield 45.0 MPaISO 527
Elongation at Break 51 %ISO 527
Flexural Strength 36.0 MPaISO 178
Izod Impact, Notched (ISO) 3.10 J/cm²1A; ISO 180
Charpy Impact Unnotched NB1 eU, 15 J; ISO 179
Charpy Impact, Notched 2.80 J/cm²1eA; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 4.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mmIEC 60243
Dissipation Factor 0.034
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.48 J/g-°C
Melting Point 167 °C10°C/min.; ISO 3146
Maximum Service Temperature, Air 100 °C
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °CISO 75
Vicat Softening Point 121 °C50 N; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 120 °CBarrel temperature
Mold Temperature 50.0 - 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 100ST BK602 POM-HI
Celanese Hostaform® XT 90 POM, Impact Modified
Celanese Hostaform® XT 20 POM, Impact Modified
Celanese Hostaform® S 9364 XAP2 ™ POM, Impact Modified
Celanese Hostaform® S 9244 XAP2 ™ POM, Impact Modified

PZAK001 / 72840

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.