Lustran® 1152 resin is a very high-impact extrusion grade of ABS (acrylonitrile butadiene styrene) with a balance of properties not offered by other grades of ABS. It offers superior toughness, particularly for low-temperature applications, and good thermoformability. Features: Very high impact strength, Superior toughness, especially in low temperature applications, Ease of coloring, Good thermoformability, UL 94 HB rated. Applications: Vehicle instrument panels, Luggage shells, Agricultural equipment, Construction equipment.Information provided by Styrolution. |