MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Mineral Reinforced

Material Notes: Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler.

Colors: Grey

Available in: Latin America

Main Properties: ? Good Mechanical Properties, Good Superficial Aspect and Dimensional stability

Applications: TECHNYL B 738 MX15 Cinza 3279 is indicated for automotive and electrical industry. Ex.: Wheel Cover

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183/A
Water Absorption 1.17 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 59.0 MPaISO R 527
Elongation at Break 3.0 %ISO R 527
Tensile Modulus 4300 MPaISO R 527
Flexural Strength 100 MPaISO 178
Flexural Modulus 3700 MPaISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 60.0 kJ/m²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 243.5 °C
 
Processing PropertiesOriginal ValueComments
Feed Temperature 250 - 260 °C
Nozzle Temperature 250 - 270 °C
Mold Temperature 80.0 - 100 °C
 
Descriptive Properties
Compression Zone260-280°C
Mixing Zone250-270°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Minlon® EFE6096 GY090A PA66-IMD15
IN-738 Cast Nickel Superalloy
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
Permabond 738 Cyanoacrylate, toughened
Nye Lubricants 738 (RL) Synthetic Oil

PRHOD750 / 137981

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.