MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess LEWATIT® K 2431 Polymer-based Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® K 2431 is a strongly acidic, macroporous, polymer-based resin in spherical bead form, with sulfonic acid groups. It is ideal suited as a heterogeneous catalyst for organic reactions In contrast to gel-type resins, the macroporous structure of this catalyst allows larger molecules better access to the active sites. This catalyst generally gives better access to the active sites. This catalyst generally gives better results when used in media of higher polarity. Lewatit K 2431 is especially designed for the following applications:
  • phenol alkylation with olefins
  • esterification, etherification, condensation and alkylation of larger polar and non-polar molecules
  • purification of phenol

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.730 g/cc0.0264 lb/in³
Density 1.15 g/cc0.0415 lb/in³
Bead Size 0.500 - 1.60 mm0.0197 - 0.0630 in>90%
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8753 / 209146

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.