MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE EE-2340DN XRD Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-2340DN XRD is a general purpose thermoplastic elastomer used in automotive applications. Sarlink EE-2340DN XRD is a high hardness grade with good UV resistance. This grade can be processed by extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: High Density; High Hardness; Low Temperature Toughness; Ozone Resistant; Sunlight Resistant; UV Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Viscosity 423 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 39
@Time 15.0 sec
Injection Molded; ISO 868
 40
@Time 5.00 sec
Injection Molded; ISO 868
 43
@Time 1.00 sec
Injection Molded; ISO 868
 40
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 41
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 41
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 42.6
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 44.2
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
 45.7
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 1710 psiFlow, Type 1, 20 in/min; ISO 37
 2190 psiAcross Flow, Type 1, 20 in/min; ISO 37
 1670 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 1700 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 1910 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 2150 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 867 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 1270 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 971 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 168 hr; ISO 188
 988 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 1490 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 1520 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 460 %Flow, Type 1, 20 in/min; ISO 37
 700 %Across Flow, Type 1, 20 in/min; ISO 37
 327 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 331 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 639 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 641 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 310 pliFlow; ISO 34-1
 400 pliAcross Flow; ISO 34-1
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
Type A; ISO 815
 59 %
@Temperature 90.0 °C,
Time 252000 sec
Type A; ISO 815
 65 %
@Temperature 70.0 °C,
Time 79200 sec
Type A; ISO 815
 79 %
@Temperature 125 °C,
Time 252000 sec
Type A; ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 450 - 490 °FMelt, Injection
Rear Barrel Temperature 450 - 490 °FInjection
Middle Barrel Temperature 450 - 490 °FInjection
Front Barrel Temperature 450 - 490 °FInjection
Nozzle Temperature 450 - 490 °FInjection
Zone 1 430 - 470 °FExtrusion
Zone 2 430 - 470 °FExtrusion
Zone 3 430 - 470 °FExtrusion
Zone 4 430 - 470 °FExtrusion
Zone 5 430 - 470 °FExtrusion
Die Temperature 430 - 470 °FExtrusion
Mold Temperature 60.0 - 90.0 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 25A, Non-Black Sulfur Cure
Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade
Wacker Elastosil® R plus 4001/30 Silicone Rubber
Teknor Apex Monprene® CP-3090D XRD Thermoplastic Elastomer
NuSil VersaSil 40 MED-4042 Silicone

PTEKNQ1039 / 237530

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.