MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vitro Minerals MG 325 Recycled Glass Powder
Categories: Ceramic; Glass

Material Notes: MG Glass powders are made from 100% recycled glass in a low-iron processing environment. They provide a clean, white-colored material that is specially selected for applications as a fluxing powder for white ceramics. X-ray diffraction and scanning electron microscopy confirm that the MG Glass powders are fully amorphous and contain no crystalline silica. Vitro Minerals’ processing system provides consistent product quality and uniform particle size distribution for two grades with finenesses covering a range of potential user requirements: MG-200 (d98 = 75 µm); MG-325 (d98 = 45 µm)

Information provided by Vitro Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/ccASTM C127
Bulk Density 55.0 lb/ft³ASTM C127
Brightness 90 - 93 %
Moisture Absorption at Equilibrium <= 0.50 %Free; ASMT C566
Particle Mesh Size 325 Mesh>90%; ASTM C136
pH 10 - 11AFS 113-87-S
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.5ASMT C566
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.00 - 3.0 %
CaO 5.0 - 14 %
Fe2O3 0.00 - 0.20 %
Loss on Ignition(%) <= 0.10 %
MgO 0.00 - 6.0 %
Na2O or K2O 10 - 18 %
Other 0.00 - 5.0 %
SiO2 69 - 74 %
 
Descriptive Properties
ColorUltra White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CVITRO914 / 209588

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.