MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Europrene® N OZO 7033 NBR-PVC blend
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Europrene® N OZO 7033 is a blend of acrylonitrile-butadiene copolymer and polyvinyl chloride in the ratio 70/30. The fluxing stage is fully achieved during the mechanical mixing thus providing outstanding resistance against ozone and good oil, abrasion and fire resistance together with an excellent processability.

Key Features: Europrene® N OZO 7033 is characterized by an excellent processability in internal and open mixers, high resistance to oils and outstanding fire resistance. This grade exhibits a good compromise between ozone resistance and low temperature performances. Particularly suitable for extrusion and injection molding applications, this grade could be vulcanized with sulphur based systems or with peroxides.

Main Applications: Conveyor belts, safety shoe soles, cable jackets, industrial and automotive hoses, flooring, fire hoses and all applications where fire and ozone resistance are required together with moderate flexibility at low temperature.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %ASTM D5668
Mooney Viscosity 75
@Temperature 100 °C
ASTM D1646
Ash <= 0.50 %ASTM D5667
 
Descriptive Properties
Acrylonitrile Content23% wtASTM D3533
NBR/PVC Ratio, wt/wt70/30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitriflex N-7411 NBR / PVC
Avient Elastamax™ HTE 3080 Polyvinyl Chloride + NBR (PVC+NBR)
Armacell Monarch® F-06232 (Natural) NBR/PVC Foam
Avient ProFlex™ MB NV866/20 Nitrile/PVC Elastomer (NBR/PVC) Compound
Nitriflex N-6420 NBR / PVC

PENG274 / 124668

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.