MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Zirconia BusterF Alumina Bulk Fiber Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Aluminum Oxide

Material Notes: Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rigid shapes, placed into cavities as loose fill insulation, or added to ceramic bodies and coatings for reinforcement. They are differentiated by fiber length but share the same fiber diameter and calcined chemical composition. Typically these fibers are 3 to 4 microns in diameter.

BusterF fibers exhibit low thermal conductivity, low thermal mass and immunity to thermal shock. A minor addition of silica modifies the fiber's microcrystalline structure and acts as a grain growth inhibitor and prevents embrittlement that usually occurs in pure alumna after extended use at elevated temperatures. BusterF fibers resist attack in aggressive chemical environments due to its high purity & refractory nature. It is stable in vacuum, inert or reducing atmospheres.

BusterF fibers yield a uniform body of 0.16 - 0.24 gm/cm3 (10-15 pcf) density, when vacuum formed from a water slurry. BusterF-10 fibers will produce higher density vacuum formed boards and cylinders. Silica, alumina and aluminum phosphate binders can be used to form rigid refractory thermal insulation products.

BusterF fiber is useful as insulation packing in furnace spaces, around furnace sight tubes & ports and fill in expansion joints and masonry cracks.

Features:

  • Available in Two Different Forms
  • Low Thermal Conductivity
  • Highly Refractory
  • Low Heat Storage
  • Extreme High Temperature Stability
  • 97% Pure Alumina
  • Lightweight
  • Available “Off the Shelf”

Information provided by Zircar Zirconia.

Key Words: Al2O3, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.40 g/ccFiber
Bulk Density 0.0800 g/ccShipping
 
Thermal PropertiesOriginal ValueComments
Melting Point 2038 °C
Maximum Service Temperature, Air 1700 °C
Shrinkage 2.0 %
@Temperature 1538 °C,
Time 3600 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 97 %
SiO2 3.0 %
 
Descriptive Properties
Alpha Alumina>50%
Approximate Fiber Length50-100 mm
Mean Fiber Diameter3.5 microns
Trace Inorganics0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1005 Steel
Zircar Zirconia ALK-15 Alumina Knit Textile Insulation
Zircar Zirconia ZYP-30 Zirconia Powder
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Zircar Zirconia ZYBF-3 Zirconia Bulk Fiber Insulation

C6ZIR042 / 2798

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.