Nistelle C is designed primarily for high corrosion resistance, and therefore used for pumps and valve parts etc. in the chemical industry, and is available both for hardfacing by welding and as castings. Nistelle C has excellent high temperature strength and resistance to oxidation, being extensively used for hardfacing drop forging dies. It is readily machinable.Information provided by Kennametal Stellite™ |