MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical XY-1076 Antioxidant
Categories: Other Engineering Material

Material Notes: This product is a highly efficient type of hindered phenol antioxidant, showing the performance of anti-discoloration caused by light and heat, and some stabilizing effect on the light, which is odorless and tasteless with stability, being soluble in benzene, acetone and esters, insoluble in water, and slightly soluble in ethanol. There is no pollution with this product that shows good extraction of heat and water resistance with good compatibility for most copolymers like PE, PP, PS, PA, POM, ABS, PVC and polymer materials such as synthetic rubber. In addition, it is also used for grease and paint against thermal aging oxidation.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.50 %
@Temperature 105 °C,
Time 7200 sec
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 50.0 - 55.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 97 %
@Wavelength 425 nm
2g/20ml toluene
 >= 98 %
@Wavelength 500 nm
2g/20ml toluene
 
Descriptive Properties
AppearanceWhite crystalline powder
Content>99%Main

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX032 / 317879

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.