MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
AGC Fluon® TL-171E Micropowder
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Product Description: Fluon® TL-171E is a white PTFE (polytetrafluoroethylene) micropowder which is easy to disperse in a wide range of liquids. The reduced total surface areas of Fluon® TL-171E minimizes viscosity increase during mixing. The particles are soft, however, and retain good film forming capability. This combination of properties makes Fluon® TL-171E very useful in coating formulations. Fluon® TL-171E is suitable for use in food contact applications.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 g/ccASTM D4894
Volatiles 0.060 %
Particle Size 4.0 µmHegman; ASTM D1210
 5.0 µmLow Shear
 9.0 µmLow Shear
 16 µmLow Shear
Specific Surface Area 2.6 m²/g
 
Thermal PropertiesOriginal ValueComments
Melting Point 331 °CASTM D3417
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM D4019
 
Descriptive Properties
Oil Absorption45 lb oil/100 lbASTM D1438
Oil Penetrometer99[1/10 mm], ASTM D1403

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAGCX285 / 191394

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.