MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds Free Form® Habitat® Cast N Coat™ Epoxy Putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: Habitat Cast N Coat™ is a filled, two component (A+B) liquid epoxy that can be cast solid or thickened for brushing on / troweling on to vertical surfaces. Material cures to a rock-hard solid with negligible shrinkage. Mix ratio is 1A:1B by volume. Working time is 85 minutes and material cures overnight (at room temperature). UVO™ or Ignite™ colorants can be added to liquid Cast N Coat™ during mixing to create a variety of color effects. Cured epoxy can be sanded and painted with acrylic paints. Habitat Cast N Coat™ certifies to the highest flame rating available (ASTM E84, Class A), making this material ideal for public space fabrication applications. Also, it does not contain VOC’s, phthalates or crystalline silica (a known carcinogen) and is safe for making elements used in proximity to animals/reptiles and aquatic life. Epoxy bonds permanently to itself or a variety of surfaces and can be applied as a fire rated protective/decorative coating to EPS or rigid foam, wallboard, plaster, wood, PVC and more. Habitat Cast N Coat™ is also an excellent repair cement and bonds permanently to itself, PVC, Plexiglas™ (acrylic), wood, many metals, plastics and foams.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D-1475
Viscosity 13500 cPMixed; ASTM D-2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D-2240
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hour
Pot Life 85.0 minASTM D-2471
 
Descriptive Properties
ColorTan
Heat Deflection Temp55°CASTM D-648
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume18.35[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN216 / 296917

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.