MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Selenis SAFE FT 104 Copolyester for Medical Markets
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Safe FT 104 is a copolyester that has been specifically developed for the production of parts suitable for medical devices. This grade is manufactured to rigorous quality standards to meet the requirements of the highly regulated medical industry. Selenis Safe FT 104 offers glass clear transparency with the advantage of being unbreakable and therefore improving the safety of laboratory operators. The use of polyester in this field has become well established. The clinical performance outperforms glass as the contamination risk is reduced, improving patients’ safety and comfort.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.800 g/cc
Density >= 1.37 g/cc
Moisture Absorption at Equilibrium <= 0.20 %
Viscosity Test 59 - 63 cm³/gIntrinsic; ISO 1628-5
Crystallinity >= 35 %ASTM D1505
ASTM Color <= 0.00b*; ASTM D6290
 >= 80L*; ASTM D6290
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 235 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Processing Temperature 265 °C
Drying Temperature 120 - 150 °C
@Time 14400 - 21600 sec
10ºC ramp every hour
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE936 / 243434

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.