MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound WF006XXL Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP THERMOCOMP WF006XXL compound is based on Polybutylene Terephthalate (PBT) resin containing 30% glass fiber. Added features of this grade include: Good Mold Release, Heat Stabilized, Low Extractables.

Features: Low Extractable,High Stiffness,Heat Stabilized,Good Mold Release,Food Contact Acceptable,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.57 g/ccASTM D792
Density 1.57 g/ccISO 1183
Moisture Absorption 0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0500 %Injection Molding
 0.0600 %23°C / 50% RH; ISO 62
Viscosity 12 cP
@Load 1.20 kg,
Temperature 265 °C
MVR cc/10 min; ISO 1133
 21 cP
@Load 2.16 kg,
Temperature 265 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0021 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0121 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 128 MPa5 mm/min; ASTM D638
 131 MPa5 mm/min; ISO 527
Elongation at Break 2.4 %5 mm/min; ISO 527
 2.7 %5 mm/min; ASTM D638
Tensile Modulus 10330 MPa5 mm/min; ASTM D638
 10449 MPa1 mm/min; ISO 527
Flexural Strength 184 MPa2 mm/min; ISO 178
 185 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8900 MPa2 mm/min; ISO 178
 9130 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 55.0 JASTM D256
Izod Impact, Unnotched 585 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 43.0 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 49.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.90 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 222 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 224 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 209 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 213 °CRate B/120; ISO 306
 214 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 260 °C
Zone 2 245 - 255 °C
Zone 3 260 - 270 °C
Melt Temperature 240 - 265 °CInjection Molding
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81958 / 289905

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.