MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
JSC SKS-30 ARKM-15 / SBR-1705 Styrene-butadiene rubber
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Description: Styrene-butadiene rubber SKS-30 ARKM-15 (SBR-1705) is a styrene and butadiene copolymer obtained by cold polymerization with the use of mixture of rosin and fatty acids soaps. The rubber is filled with DAE-type extender oil for synthetic rubbers.

REACH: registered

Application: SKS-30 ARKM-15 (SBR-1705) is a general-purpose rubber, widely used in industrial rubber and cable industries. Appearance: briquettes (bales)

Color: from light-brown to dark-brown

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.60 %
@Time 3600 sec
ASTM D5668 (method C)
Mooney Viscosity <= 6.0spread within a batch
 45 - 54
@Temperature 100 °C
ML 1+4; ASTM D1646 (para. 7.2.2)
Ash <= 0.60 %ASTM D 5667 (part A)
Storage Temperature <= 30.0 °C
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22 - 25 %Bound; ASTM D5775
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 21.6 MPaASTM D 412 method A
Tensile Stress >= 10.8 MPa
@Strain 300 %
ASTM D 412 method A
Elongation at Break >= 400 %ASTM D 412 method A
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Content<0.25%Organic acids soaps, ASTM D5774
 0.15-0.35%Antioxidant VS-1 (CAS # 9003-36-5)
 14-17%Oil (DAE), ASTM D 5774
 19-25%Solvent extract, ASTM D5774
 4.8-6.4%Organic acids, ASTM D5774
Rheometric Properties1.4-3.4 dNmML, ASTM D 5289
 12-20 mint90, ASTM D 5289
 13-20 dNmMH, ASTM D 5289
 2.5-6 mints1, ASTM D 5289
 6.5-11.5 mint50, ASTM D 5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSC010 / 317830

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.