MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema Rilsan® Clear G170 Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical uses.

Information provided by Arkema Group

Property data for dry samples, unless noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
 1.05 g/ccCond.; ISO 1183
Water Absorption 3.8 %Dry; Sim. to ISO 62
Moisture Absorption 1.70 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cmDry; ISO 294-4, 2577
 0.0070 cm/cm
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield 74.0 MPaCond.; ISO 527-1/-2
 76.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 8.0 %Dry; ISO 527-1/-2
 9.0 %Cond.; ISO 527-1/-2
Tensile Modulus 2020 MPaCond.; ISO 527-1/-2
 2100 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmCond.; IEC 60093
Surface Resistance 1.00e+12 ohmCond.; IEC 60093
Dielectric Strength 50.0 kV/mmCond.; IEC 60243-1
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°CDry; ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °CDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 136 °CDry; ISO 75-1/-2
Vicat Softening Point 160 °C50°C/h 50N; Dry; ISO 306
Glass Transition Temp, Tg 168 °C10°C/min; Dry; ISO 11357-1/-2
Flammability, UL94 V-2
@Thickness 1.60 mm
Yellow Card Available; Dry; IEC 60695-11-10
Oxygen Index 26 %Dry; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 91 %Luminous; ISO 13468-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
Hold Pressure 19.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveYes
Processing MethodsInjection Molding
 Other Extrusion
TransparentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techno Polymer Techno ABS LM100 Transparent
EMS-Grivory Grilamid® TR 55 PA12/MACMI
Envalior Novamid® 3010SR NAT PA66
Covestro Makroblend® M525 PC+PET
A. Schulman Diamond ABS TR-5000 Transparent

PARKG652_a / 149070

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.