(Viewing data as-entered.
Click here
to return)
Polyram RamShine PV300G6 ABS, 30% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Material Notes:
30% glass fiber reinforced, heat resistance and minimal mold shrinkage ABS for injection molding applications
Information provided by Polyram Ram On Ind.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.28
g/cc
DIN 53479
Water Absorption
0.12 %
DIN 53495
Linear Mold Shrinkage
0.0010
-
0.0020
cm/cm
Melt Flow
8.0
g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
115
ASTM-D785
Tensile Strength, Yield
90.0
MPa
ASTM-D638
Elongation at Break
3.0 %
ASTM-D638
Flexural Strength
115
MPa
ASTM-D790
Flexural Modulus
8.00
GPa
ASTM-D790
Izod Impact, Notched
0.800
J/cm
@Temperature 23.0 °C
ASTM-D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+16
ohm-cm
DIN 53482
Surface Resistance
1.00e+14
ohm
DIN 53482
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
101
°C
DIN 53461
Flammability, UL94
HB
@Thickness 3.00 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Polyram RamShine PV300G4 ABS, 20% Glass Fiber
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Covestro Makrolon® 6485 Polycarbonate, Injection Grade
Covestro Makrolon® 6385 Polycarbonate, Injection Grade
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
PPOLYRA363 / 57625
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.