MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECACOMP PP ID blue 1049775 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
  • metal detectable
  • x-ray detectable
  • Explanation of food contact according to FDA and EU 10/2011 on request

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.34 g/cc
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 22.0 MPaDIN EN ISO 527-1
Elongation at Break 16 %DIN EN ISO 527-1
Modulus of Elasticity 1.60 GPaDIN EN ISO 527-1
Charpy Impact Unnotched 21.0 kJ/m²DIN EN ISO 179-1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °C
Maximum Service Temperature, Air 100 °Clong term
 130 °Cshort term
Glass Transition Temp, Tg 13.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 260 °CCylinder
Melt Temperature 230 - 250 °CMaterial temperature
Mold Temperature 40.0 - 100 °C
Drying Temperature 70.0 - 100 °C
Dry Time 2.00 hour
 
Descriptive Properties
Colorblue
Detectability3.0 mm Al4 x 4 x 4 mm, x-ray detectable
 4.0 mm Al4 x 4 x 4 mm, metal detectable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO9116 / 319044

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.