MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QGel 314 General Purpose Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QGel 314 is a two-part, highly tacky, translucent, liquid silicone gel, which cures at elevated temperatures. This product is supplied in matched kits in a 10:1 ratio of A:B. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.

Key Features:

  • Convenient 10:1 mixing ratio for use in automatic dispensing equipment or hand mixing
  • High tack surface
  • High strength tough gel

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccUncatalyzed B
 1.01 g/ccUncatalyzed A
Viscosity 3500 cPUncatalyzed B
 65000 cPUncatalyzed A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 25
@Treatment Temp. 150 °C,
Time 1800 sec
Cured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 150 °C
 45.0 min
@Temperature 100 °C
 60.0 min
@Temperature 80.0 °C
Gel Time 120 minCatalyzed
 
Descriptive Properties
ColorTransparentUncatalyzed A
 TransparentUncatalyzed B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QGel 319 Optically Clear Silicone Gel
CHT Group QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group QGel 312 Custom Silicone Gel
CHT Group QGel 311 UV Special Purpose Silicone Gel
CHT Group QGel 317 General Purpose Silicone Gel

PACC2016 / 199404

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.