Function: Used as a processing promoter in rubber compounds based on natural and synthetic rubbers Application: Eraser rubber compounds (can also be hot cured with basic accelerators), cold-cured goods such as light-colored calendered sheathing and rubber-coated fabrics. Information provided by Lanxess. |