SupremEX® 225XE is a high quality aerospace grade aluminum alloy (AA2124) that offers a high tensile modulus approximately 60 percent higher than the parent alloy and slightly higher than that of titanium. It also offers good strength, excellent fatigue characteristics and is particularly well suited for applications demanding a good balance of properties. PGQ = Poly-Glycol Quench Information supplied by Materion. |
AlSiC. Designation: – 2124/SiC/25p |