MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Deutsche Titan Tikrutan LT 34 Alloyed Titanium  (discontinued **)
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Tikrutan LT titanium alloys are used where the mechanical properties of the commercially pure or low-alloyed titanium materials do not meet the requirements of the application. Thanks to their high strength-to-density ratio as compared with steel these alloys make for appreciable weight savings, which e.g. in the aerospace industry are essential. In many cases titanium alloys are the only conceivable material for engineering components which are subjected to severe acceleration forces and have to be highly durable to maintain the performance of the plant.

Used in aerospace, auto, and medical engineering industries.

Information provided by Deutsche Titan

TiAl4Mo4Sn2Si; DIN 3.7185; WL 3.7184; BS TA 48-51, TA 57; AIR TA4D4E; AECMA Ti-P63001

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 350
@Thickness 6.00 - 25.0 mm
HB 30; Annealed
Tensile Strength, Ultimate 1100 - 1280 MPa
@Thickness 6.00 - 25.0 mm
Aged
Tensile Strength, Yield >= 870 MPa
@Thickness 100 - 150 mm
Aged
 >= 920 MPa
@Thickness 25.0 - 100 mm
Aged
 >= 960 MPa
@Thickness 6.00 - 25.0 mm
Aged
Elongation at Break >= 9.0 %
@Thickness 100 - 150 mm
Aged
 >= 9.0 %
@Thickness 25.0 - 100 mm
Aged
 >= 9.0 %
@Thickness 6.00 - 25.0 mm
Aged
 >= 9.0 %
@Thickness 6.00 - 25.0 mm
Annealed
Reduction of Area >= 20 %
@Thickness 100 - 150 mm
Aged
 >= 20 %
@Thickness 25.0 - 100 mm
Aged
 >= 20 %
@Thickness 6.00 - 25.0 mm
Aged
Modulus of Elasticity 117 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000150 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.60 µm/m-°C
@Temperature 250 °C
Thermal Conductivity 7.50 W/m-K
@Temperature 20.0 °C
Transformation Temperature 975 °Cß/(α+ß)
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.0 - 5.0 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.20 %
Molybdenum, Mo 3.0 - 5.0 %
Nitrogen, N <= 0.050 %
Oxygen, O <= 0.25 %
Silicon, Si 0.30 - 0.70 %
Tin, Sn 1.5 - 2.5 %
Titanium, Ti 86.205 - 92.2 %
 
Descriptive Properties
Phase Typeα+ßAt Room Temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed
Deutsche Titan Tikrutan RT 12 Commercially Pure Titanium
Deutsche Titan Tikrutan RT 15 Commercially Pure Titanium
Deutsche Titan Tikrutan RT 18 Commercially Pure Titanium

NDEUTI15 / 16111

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.