MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
414 Stainless Steel, annealed and cold drawn bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Key Words: UNS S41400, AMS 5615, ASTM A276, ASTM A314, ASTM A473, ASTM A511, ASTM A580, FED QQ-S-763, SAE J405 (51414), martensitic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 235
Hardness, Rockwell B 97Converted from Brinell
Hardness, Rockwell C 21Converted from Brinell
Hardness, Vickers 247Converted from Brinell
Tensile Strength, Ultimate 795 MPa
Tensile Strength, Yield 620 MPa
@Strain 0.2 %
Elongation at Break 20 %in 50 mm
Tensile Modulus 200 GPa
Izod Impact 30.0 - 80.0 Jhardened and tempered
 70.0 - 110 Jannealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000700 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µm/m-°C
@Temperature 0.000 - 100 °C
 11.0 µm/m-°C
@Temperature 0.000 - 315 °C
 12.1 µm/m-°C
@Temperature 0.000 - 540 °C
 12.4 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 24.9 W/m-K
@Temperature 100 °C
 28.7 W/m-K
@Temperature 500 °C
Melting Point 1425 - 1480 °C
Solidus 1425 °C
Liquidus 1480 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 12.5 %
Iron, Fe 83 %
Manganese, Mn <= 1.0 %
Nickel, Ni 1.88 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
420 Stainless Steel, annealed bar
AISI Type 316F Stainless Steel, annealed bar
414 Stainless Steel, annealed plate
416 Stainless Steel, annealed bar
AISI Type 316L Stainless Steel, annealed bar

MQ414N / 13026

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.