MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
ITW Insulcast® 136 Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 136 is an easy to use epoxy casting/potting compound exhibiting excellent adhesion to metals, ceramics and most plastics. When properly cured with INSULCURE 11B, INSULCAST 136 will conform to the requirements of MIL-I-16923, Types B, C & D, and will not support fungusgrowth.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccUncured. Insulcure 11B
 0.970 g/ccUncured. Insulcure 9
 1.59 g/ccUncured. Insulcast 136
Viscosity 55 cPInsulcure 9; ASTM D2393
 700 cPInsulcure 11B; ASTM D2393
 25000 cPInsulcure 11B; ASTM D2393
 30000 cPInsulcure 9; ASTM D2393
 80000 cPInsulcast 136; ASTM D2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87cured. Insulcure 9; ASTM D2240
 89cured. Insulcure 11B; ASTM D2240
Tensile Strength 10000 psicured. Insulcure 9; ASTM D638
 10200 psicured. Insulcure 11B; ASTM D638
Elongation at Break 2.0 - 4.0 %Cured. Insulcure 11B; ASTM D638
 2.0 - 4.0 %Cured. Insulcure 9; ASTM D638
Flexural Strength 15500 psiCured. Insulcure 9; ASTM D790
 17000 psiCured. Insulcure 11B; ASTM D790
Compressive Strength 15000 psiCured. Insulcure 9; ASTM D695
 15500 psiCured. Insulcure 11B; ASTM D695
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+16 ohm-cmInsulcure 11B; ASTM D150
 5.00e+16 ohm-cmInsulcure 9; ASTM D150
Dielectric Constant 4.8
@Frequency 1000 Hz
Insulcure 11B; ASTM D150
 4.8
@Frequency 1000 Hz
Insulcure 9; ASTM D150
Dielectric Strength 440 V/milInsulcure 11B; ASTM D149
 440 V/milInsulcure 9; ASTM D149
Dissipation Factor 0.020
@Frequency 1000 Hz
ASTM D150
 0.020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°CCured. Insulcure 11B
 40.0 µm/m-°CCured. Insulcure 9
Thermal Conductivity 5.00 BTU-in/hr-ft²-°FCured. Insulcure 11B
 5.00 BTU-in/hr-ft²-°FCured. Insulcure 9
Maximum Service Temperature, Air 105 °CInsulcure 9
 155 °CInsulcure 11B
Heat Distortion Temperature 80.0 °CLoad Not Reported. Insulcure 9
 155 °CLoad Not Reported. Insulcure 11B
Shrinkage 0.20 %Cured. Insulcure 9
 0.20 %Cured. Insulcure 11B
 
Processing PropertiesOriginal ValueComments
Pot Life 30.0 min
@Temperature 25.0 °C
Insulcure 9
 150 min
@Temperature 25.0 °C
Insulcure 11B
Shelf Life 12.0 MonthInsulcast 136
 12.0 MonthInsulcure 11B
 12.0 MonthInsulcure 9
 
Descriptive Properties
ColorAmberUncured. Insulcure 9
 AmberUncured. Insulcure 11B
 BlackUncured. Insulcast 136
Mix Ratio by weight100:6-7Insulcast 136:Insulcure 9
 100:9-10Insulcast 136:Insulcure 11B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9098 / 239608

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.