Designation ISO 1874-PA11,M,18-020,GB30 Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free. Outstanding isotropic properties. High compressive strength. Low and homogeneous shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Water potable contact approval WRC 950 1509. UL classification: UL94 HB RTI(C) 65/65/65 Example applications: Mechanical parts with high dimensional precision. Information provided by Arkema. |