MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ExxonMobil Oppalyte™ 30 HM-3 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A white opaque OPP film with a proprietary cavitated core. HM-3 is designed for cold seal applications and is used as a surface print, monoweb, or as the inside of lamination. It is non-sealable film.

Availability: Latin America, North America and South America

Key Features:

  • Excellent stiffness and flex resistance
  • Outstanding opacity
  • Bright white appearance
  • Very good moisture barrier
  • Excellent print performance for flexographic and rotogravure printing
  • The treated cold seal layer provides exceptional cold seal adhesion, with very good adhesion to synthetic cold seals
  • The treated cold seal layer allows for back-side printing with FDA approved inks.
Features:
  • Light Barrier
  • Moisture Barrier
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Ice Cream
Uses:
  • HFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.350 g/100 in²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Thickness 1.20 milExxonMobil Method
Coating Weight 12.5 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Break, MD 12300 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 26000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 5.0 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Gloss 60 %45°, Print Surface; ExxonMobil Method
Transmission, Visible 34 %ExxonMobil Method
 
Descriptive Properties
Opacity0.78
Wetting Tension0.80 receding cos theta
 0.90 receding cos theta
Yield35400 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX99496 / 175732

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.