MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Trinseo MAGNUM™ 3904 Smooth LP ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Product Description: MAGNUM™ 3904 Smooth LP is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology ensures an ABS resin that combines excellent processability with a stable light base color that is ideal for self-coloring. With its ultra-low particulate content, this grade is an addition to the “smooth Series” and features a lower plate (LP) out content. This results in a superior surface finish in which the plate out build-up on the extruder roll stack is reduced significantly. This new grade enables customers to produce parts with both outstanding aesthetics and surface cleanness at lower total cost.
Applications: Automotive interior; Furniture

Availability: Europe; North America

Features: Good Processability; Good Surface Finish; High Impact Resistance; Platable

Uses: Furniture

Form: Pellets

Processing Method: Extrusion; Thermoforming

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 g/ccISO 60
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 4.7 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5370 psiISO 527-2/50
Elongation at Yield 2.6 %ISO 527-2/50
Tensile Modulus 264000 psiIOS 527-1/1
Flexural Strength 8410 psiISO 178
Flexural Modulus 276000 psiISO 178
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 207 °FUnannealed; ISO 75-2/A
Vicat Softening Point 207 °FISO 306/B50
Flammability, UL94 HB
@Thickness 1.52 mm
 
Processing PropertiesOriginal ValueComments
Drying Temperature 176 - 194 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1538 / 312231

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.