MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Solvay A6000 ETFE Fluoropolymer Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Description: Release film. Ideally suited to debulking applications.

Features & Benefits:

  • High temperature, tough fluoropolymer release film with excellent release characteristics combined with high elongation
  • Suitable for use with all commonly used resin systems
  • Clear blue for ease of identification on the cured laminate

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/cc
Thickness 12.0 microns
 15.0 microns
 20.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6106 - 10152 psi
Elongation at Break 350 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °C
 
Descriptive Properties
ColorClear blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RC-3000-NB Breather fabric
Solvay AB40N Breather fabric
Solvay BR100 Nylon fabric
Solvay RC-3000-10 Breather fabric
Solvay RC-3000HT Breather fabric

PCYTED283 / 180585

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.