MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pressure Seal 14801 Chlorosulfonated
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 14801 is a 70 durometer black colored general purpose Hypalonelastomer. It has good physicals and exhibits good resistance to synthetic lubricating oils.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 CE 715; 3 CE 715 B15

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
 50
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #3
 59
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 67
@Temperature 150 °C,
Time 252000 sec
Service Fluid 100
 67
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 69
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 71
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 73
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #1
 81
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 84
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 84
@Temperature 150 °C,
Time 252000 sec
Heat Aged
Tensile Strength 3152 psi
 992.9 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 992.9 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1468.8 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 2215.9 psi
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #3
 2792.7 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 2868.3 psi
@Temperature 150 °C,
Time 252000 sec
Service Fluid 100
 3224.5 psi
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 3328.5 psi
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #1
 3391.6 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 3391.6 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 259 %
 50 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 50 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 129 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 175.1 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 175.1 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 196.1 %
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #1
 212.9 %
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #3
 220.9 %
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 229.5 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 246.05 %
@Temperature 150 °C,
Time 252000 sec
Service Fluid 100
100% Modulus 724 psi
Tear Strength 204 pliDie B
Compression Set 15.3 %
@Temperature 70.0 °C,
Time 79200 sec
Solid
 73.6 %
@Temperature 125 °C,
Time 79200 sec
Solid
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -51.0 °F
Shrinkage -5.10 %
@Temperature 150 °C,
Time 252000 sec
Volume, Heat Aged
 -5.10 %
@Temperature 150 °C,
Time 252000 sec
Volume, Heat Aged, Test Tube Method
 -4.00 %
@Temperature 125 °C,
Time 252000 sec
Volume, Heat Aged, Test Tube Method
 -4.00 %
@Temperature 125 °C,
Time 252000 sec
Weight, Heat Aged
 2.5 %
@Temperature 125 °C,
Time 252000 sec
Volume, ASTM Oil #1
 7.7 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 9.2 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 10.5 %
@Temperature 150 °C,
Time 252000 sec
Volume, Service Fluid 100
 53.5 %
@Temperature 125 °C,
Time 252000 sec
Volume, ASTM Oil #3
 53.8 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL093 / 318303

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.