MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Elastamax™ XL-0257-1 TPU-Based Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color: Grey.

Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 113 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 525 sec. delay; ASTM D2240
Tensile Strength, Ultimate 23.8 MPa10 in/min; ASTM D412
Elongation at Break 370 %10 in/min; ASTM D412
50% Modulus 0.00903 GPa
@Strain 50 %
10 in/min; ASTM D412
100% Modulus 0.0111 GPa
@Strain 100 %
ISO 37
200% Modulus 0.01455 GPa
@Strain 200 %
10 in/min; ASTM D412
300% Modulus 0.01951 GPa
@Strain 300 %
10 in/min; ASTM D412

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane

PHG880 / 47003

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.