System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Dow INSPIRE™ D7025 Polypropylene
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
High Flow, High Modulus, Paintable
Information provided by Dow
Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.09
g/cc
ISO 1183
Filler Content
25 %
ISO 3451
Melt Flow
24
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore D
69
ISO 868
Tensile Strength, Yield
21.0
MPa
ISO R527
Flexural Modulus
1.98
GPa
ISO 178
Izod Impact, Notched (ISO)
32.0
kJ/m²
ISO 180/1A
Impact Test
35.0
J
6.7 m/s, 100% ductile failure; ASTM D3763
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
121
°C
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
64.0
°C
ISO 75
Descriptive Properties
Five Finger Scratch N
3
FLTM BN 108-13
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer
Dow Engage® 8200 Polyolefin Elastomer
Dow INSPIRE™ TF2300 Polypropylene
Dow INSPIRE™ 404 Performance Polymer
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
PDOW1141 / 30345
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.