MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex APEX® 310 Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Oil Resistant

Uses:Flexible Cord Jacketing; Liquid Tight Conduit Jacketing

Wire Types:SJT; SRDT; ST

Agency Rating:UL 360

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 2780 psiASTM D638
 2780 psi
@Treatment Temp. 37.8 °C,
Time 605000 sec
Oven Aged; UL 1581
 2840 psi
@Treatment Temp. 15.6 °C,
Time 605000 sec
ASTM #2 Oil; UL 1581
Elongation at Break 340 %ASTM D638
 269 %
@Treatment Temp. 15.6 °C,
Time 605000 sec
ASTM #2 Oil; UL 1581
 340 %
@Treatment Temp. 37.8 °C,
Time 605000 sec
Oven Aged; UL 1581
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 176 °FContinuous; ASTM D794
Brittleness Temperature -11.2 °FASTM D746
Oxygen Index 25 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 °F
 
Descriptive Properties
AppearanceOpaque
Temperature Rating80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0175 / 236666

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.