MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GBC Grade 97 Alumina  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Data provided by the manufacturer, GBC Materials Corporation.

GBC Materials Corporation has been acquired by Morgan Advanced Ceramics.

Key Words: Al2O3, GBC Materials Corporation, aluminium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.72 g/cc
Open Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Tensile Strength, Ultimate 210 MPa
Flexural Strength 380 MPa
Compressive Strength 2000 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 3.10e+12 ohm-cm
Dielectric Constant 9.4
Dissipation Factor 0.00020
Dielectric Loss Index 0.013
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.60 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 1650 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 97 %
 
Descriptive Properties
ColorWhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NAPCO White Fused Alumina
Ferro Aluminum Oxide Grinding Media P87
Commercial Bronze, UNS C22000 (90-10 Bronze), H08 Temper flat products
Commercial Bronze, UNS C22000 (90-10 Bronze), H06 Temper flat products
Cadmium Aluminum Selenide, CdAl2Se4

CG0005 / 888

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.