MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay ALKAQUAT® DMB-451 80% Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: Alkyl Dimethyl Benzyl Ammonium Chloride

CAS: 68424-85-1

Water Solubility: Soluble

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ALKAQUAT© DMB-451 80% is a quaternary biocide and corrosion inhibitor. ALKAQUAT© DMB-451 80% is used in areas such as oil field and industrial applications. In addition to being a corrosion inhibitor, it also has typical surfactant properties that may be a benefit in a given formulation (i.e. wetting, surface tension reduction, particulate dispersion, etc.) Breaker, Corrosion inhibitor, Detergent, Dispersant, Emulsifier, Foam control agent, Gellant, Scale Control, Shale stabilizer, Solvent

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/cc
pH 6.0 - 9.010% Solution; RP-0420
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 15 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear Liquidat 22°C, RP-0064
 Colorless to Pale Yellow Liquid
CompositionActive80-83% (EQ. WT. 359.6), RP-0025
OdorAlcohol-like

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shale
Sandstone, Medium
Reade Advanced Materials Iron Chromite (FeO·Cr2O3)
Limestone
Flint

WRHOD061 / 137292

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.