Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System. Gel, Torque, and Dispersion were measured on a 100 phr S1025A / 20 phr V0022G Syncure System. Cured for 6 hours in water at 90°C for Gel test. Torque is > 1400. Dispersion is Visual. Pellet appearance is 1/8 round. Information provided by PolyOne |