System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Precision Polymer Engineering F80R Fluorosilicone Rubber
Categories:
Polymer
;
Thermoset
;
Fluoropolymer, TS
;
Thermoset Fluoroelastomer
;
Rubber or Thermoset Elastomer (TSE)
;
Silicone
Material Notes:
Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.
Applications:
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Hardness, Shore A
82
°IRHD; ASTM D1415
87
°IRHD, +5 change after 336 hours @ 200°C; ASTM D1415
Tensile Strength, Yield
4.55
MPa
-30% change after 336 hours @ 200°C; ASTM D412
6.50
MPa
ASTM D412
Elongation at Break
82.96 %
-32% change after 336 hours @ 200°C; ASTM D412
122 %
ASTM D412
Compression Set
14 %
@Temperature 150 °C,
Time 86400 sec
ASTM D395
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
250
°C
Minimum Service Temperature, Air
-65.0
°C
-50.0
°C
Temperature at which modulus shall not exceed 70 Mpa
Flash Point
>=
300
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPRECI142 / 57866
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.