MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Mobil Delvac 5W-40 1
Categories: Fluid; Lubricant

Material Notes: Mobil Delvac 1 5W-40 is a fully synthetic supreme performance heavy duty diesel engine oil that helps extend engine life while providing long drain capability and fuel economy for modern diesel engines operating in severe applications.  Mobil Delvac 1 utilizes state-of-the-art technology to deliver exceptional performance in modern low emission engines, including refrigerated units, as well as older, well-maintained engines. Mobil Delvac 1 5W-40 is recommended for use in a wide range of heavy-duty applications and operating environments found in the on-road transport and off-road mining, construction, and agricultural industries.  Mobil Delvac 1 also meets the API SL specification for gasoline engines used in mixed fleets.

On-highway engines operating in both high speed/high load and stop-and-go conditions; Off-highway engines operating in severe low speed/heavy load conditions; Virtually all diesel powered equipment from American, European, and Japanese equipment builders; High performance gasoline engines and mixed fleets; Refrigeration units

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.854 g/cc
@Temperature 15.0 °C
ASTM D4052
Viscosity Measurement 151Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 102 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 14.8 cStASTM D445
Ash 1.35 %Sulfated Ash, wt%; ASTM D874
 
Chemical PropertiesOriginal ValueComments
Total Base Number 12mg KOH/g; ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -45.0 °CASTM D97
Flash Point 226 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON000 / 75425

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.