MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ganpati Exim MBTS (DM)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C14H8N2S4

White of light yellow powder with slightly bitter taste, nonpoisonous. Specific gravity : 1.45-1.54. Melting point: over 160 o C. Soluble in chloroform, slightly soluble in benzene, ethyl alcohol and carbon tetrachloride, insoluble in gasoline, water and ethyl acetate. Stable in storage.

Application : The product is an accelerator of NR and SR. It has level and middle cure rate and higher Vulcanization temperature. It operates safely, disperses easily and does not contaminate, it is aging resistant. Mainly used in manufacture of tires, rubber goods. Accelerator MBTS works as plasticizer and delayed action activator in polychoroprene.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 - 1.54 g/cc
Molecular Weight 332.5 g/mol
Ash <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 166 °C
 
Descriptive Properties
AppearanceWhite or light yellow powder
Heating Loss<0.4%
Residue<0.1%150µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI065 / 317349

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.